角钢耗能自复位混凝土框架节点的耗能性能
作者:
作者单位:

1.东莞市大业施工图审查有限公司,广东 东莞523000;2.重庆大学 土木工程学院,重庆400045

作者简介:

贺成(1982- ),男,高级工程师,主要从事混凝土结构研究,E-mail:2638084759@qq.com。
HE Cheng (1982- ), senior engineer, research interest: concrete structure, E-mail: 2638084759@qq.com.

通讯作者:

简斌(通信作者),男,博士,教授,E-mail:jianbin0215@163.com。

中图分类号:

TU377.9

基金项目:

国家自然科学基金(51878100)


Energy dissipation performance of self-centering concrete frame joint with energy-dissipation angle steel
Author:
Affiliation:

1.Dongguan Daye Construction Drawings Review Co., Ltd., Dongguan 523000, Guangdong, P. R. China;2.School of Civil Engineering, Chongqing University, Chongqing 400045, P. R. China

Fund Project:

National Natural Science Foundation of China (No. 51878100)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    提出角钢耗能自复位混凝土框架设计方法,建立节点的有限元数值模型,并试验验证其有效性。对抗弯承载力比φdes预应力筋不同的节点进行模拟分析,研究其在地震作用下的自复位性能、耗能能力和材料损伤等性能指标。为提高该类节点耗能能力,通过改变角钢竖肢螺杆标距做进一步研究。结果表明:角钢耗能节点具有良好的自复位性能,但耗能能力不足;减小抗弯承载力比φdes,自复位能力降低、残余变形加大,但耗能能力增强。与混合连接节点相比,应适当降低节点抗弯承载力比φdes的最低取值,以弥补其耗能能力的不足。角钢竖肢塑性变形是节点的主要耗能方式,且集中在竖肢的螺栓孔高度和竖肢转角位置;减小竖肢螺杆标距,且保持材料其他参数不变,将导致抗弯承载力比φdes减小、截面抗弯承载力提高,节点耗能能力将随之增强。

    Abstract:

    Design method was proposed for self-centering concrete frame joints with energy-dissipation angle steel in this study. Finite element numerical model was established and its validity was verified by experiments. After the joints with different prestressed moment capacity ratios φdes were simulated, the energy dissipation capacity, self-centering performance and material damage under earthquake were studied. Changing the screw gauge distance of angle vertical leg, the measures to improve its energy-consumption capacity were further explored. The results show that the angle energy-consuming joints have perfect self-centering performance, but the energy consuming capacity is slightly insufficient. As the value of φdes decreases, the residual deformation increases and the self-centering ability decreases, but the energy dissipation capacity increases. Therefore, compared with the hybrid connection joint, the minimum φdes value of joint should be appropriately reduced to make up for its insufficient energy dissipation. The plastic deformation of the angle vertical leg is the main energy dissipation mode of the joint, concentrating on the height of the bolt hole and the turning of the vertical leg. If the distance between the vertical screws is reduced and the other material parameters keeps constant, it will lead to decrease in φdes values, increase of the bending capacity of the section and growth of the energy dissipation capacity of the joint.

    参考文献
    相似文献
    引证文献
引用本文

贺成,简斌,吴昕,吴盼.角钢耗能自复位混凝土框架节点的耗能性能[J].土木与环境工程学报(中英文),2023,45(3):90-98. HE Cheng, JIAN Bin, WU Xin, WU Pan. Energy dissipation performance of self-centering concrete frame joint with energy-dissipation angle steel[J]. JOURNAL OF CIVIL AND ENVIRONMENTAL ENGINEERING,2023,45(3):90-98.10.11835/j. issn.2096-6717.2021.097

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2021-03-05
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2023-04-29
  • 出版日期: