    Abstract:

    With the rise of ultra-high performance concrete (UHPC), researches show that UHPC as connection elements in components can improve the performance of the overall structures. The bond strength of the joint interface has drawn increasing attention worldwide. However, there is limited information on the effect model of the interfacial properties between UHPC and normal concrete. In present study, by summarizing existing experimental results and comparing experimental methods on the basis of extensive literature research, three interfacial cohesion values with different roughness were obtained (i.e. 2.24 MPa, 2.37 MPa and 2.66 MPa), with friction coefficient of 1.42, 1.63 and 1.64, respectively. The friction coefficient calculated by direct tension test was generally larger than that obtained by splitting or bending test. The formula of UHPC-NC interface bonding strength based on cohesion and shear strength was proposed. Based on traction-separation model, a 3D finite element model suitable for tensile-dominated components and compressed-shear-dominated components was established. The cohesion and contact damage parameters suitable for smooth, medium rough and rough interface were proposed. Several finite element models of the experiments in past literature were established to verify the validity of the proposed traction-separation parameters. The finite element calculation and experimental results were well fitted, which can provide reference for later FEM study.

    Reference
    [1] 张哲. 钢-配筋UHPC组合桥面结构弯曲受拉性能研究[D]. 长沙:湖南大学, 2016. Zhang Z. Bending behaviors of composite bridge deck system composed of OSD and reinforced UHPC layer[D]. Changsha:Hunan University, 2016.(in Chinese)
    [2] Blais P Y, Couture M. Precast, prestressed pedestrian bridge world's first reactive powder concrete structure[J]. PCI Journal, 1999, 44(5):60-71.
    [3] Hajar Z, Lecointre D, Simon A, et al. Design and construction of the world first ultra-high performance concrete road bridges[C]//Proceedings of the Proceedings of the International Symposium on UHPC, Kassel, Germany, Schmidt, M, 2004:39-48.
    [4] Graybeal B A. UHPC in the U.S. highway transportation system[C]//Proceedings of the 2nd International Symposium on Ultra High Performance Concrete, Kassel, Germany, F, 2008:11-17.
    [5] Rebentrost M, Wight G. Experience and applications of ultra-high performance concrete in Asia[C]//Proceedings of the 2nd International Symposium on Ultra High Performance Concrete, Kassel, Germany, 2008.
    [6] Freytag B, Heinzle G, Reichel M, et al. WILD-bridge scientific preparation for smooth realization[C]//Proceedings of Hipermat 2012 3rd international symposium on UHPC and nanotechnology for high performance construction materials. Kassel University Press, Kassel, 881-888.
    [7] 李晨光, 安明喆, 都清. 超高性能结构混凝土材料工程化应用基础研究[J]. 混凝土世界, 2010(3):28-33. Li C G, An M Z, Du Q. Basic study of engineering application of super-high performance structure concrete material[J]. China Concrete, 2010(3):28-33. (in Chinese)
    [8] 邵旭东, 胡建华. 钢-超高性能混凝土轻型组合桥梁结构[M]. 北京:人民交通出版社, 2015. Shao X D, Hu J H. The steel-UHPC lightweight composte bridge structures[M]. Beijing:China Communications Press, 2015. (in Chinese)
    [9] 曹君辉. 钢-薄层超高性能混凝土轻型组合桥面结构基本性能研究[D]. 长沙:湖南大学, 2016. Cao J H. Research on basic performance of steel-thin UHPC lightweight composite deck[D]. Changsha:Hunan University, 2016.(in Chinese)
    [10] Graybeal B A. Behavior of field-cast ultra-high performance concrete bridge deck connections under cyclic and static structural loading[J/OL]. National Technical Information Service accession PB2011-101995. McLean, VA:FHWA. http://www.trb.org/AnnualMeeting/AnnualMeeting.aspx.
    [11] Perry V, Dykstra D, Murray P, et al. Innovative field cast uhpc joints for precast bridge systems-3-span live load continuous[C]//2010 Annual Conference of the Transportation Association of Canada:Adjusting to New Realities, TAC/ATC 2010, Halifax, NS, Canada, 26-29 September 2010.
    [12] Aaleti S, Petersen B, Sritharan S. Design guide for precast uhpc waffle deck panel system, including connections[R]. Washington, D.C.:Federal Highway Administration, 2013.
    [13] Graybeal B, Ultra-high-performance concrete connections for precast concrete bridge decks[J]. PCI Journal, 2014, 59(4):48-62.
    [14] 邵旭东, 管亚萍, 晏班夫. 预制超高性能混凝土π形梁桥的设计与初步试验[J]. 中国公路学报, 2018, 31(1):46-56. Shao X D, Guan Y P, Yan B F. Design and preliminary experiments of UHPC π-shaped girder bridge[J]. China Journal of Highway and Transport, 2018, 1(31):46-56. (in Chinese)
    [15] 管亚萍. 预制超高性能混凝土π形梁桥的设计与初步试验[D]. 长沙:湖南大学, 2016. Guan Y P. Design and preliminary experiments of UHPC π-shaped girder bridge[D]. Changsha:Hunan University, 2016. (in Chinese)
    [16] Pan W H, Fan J S, Nie J G, et al. Experimental study on tensile behavior of wet joints in a prefabricated composite deck system composed of orthotropic steel deck and ultrathin reactive-powder concrete layer[J]. Journal of Bridge Engineering, 2016, 21(10):04016064.
    [17] 邵旭东, 陈斌, 周绪红. 钢-RPC轻型组合桥面结构湿接头弯曲试验[J].中国公路学报, 2017, 30(3):210-217. Shao X D, Chen B, Zhou X H. Experiment on bending behavior of wet joints in light-weighted composite deck system composed of steel and rpc layer[J]. China Journal of Highway and Transport, 2017, 30(3):210-217. (in Chinese)
    [18] 陈贝. 预制NSC构件的UHPC湿接缝受弯性能研究[D]. 长沙:湖南大学, 2018. Chen B. The Research on flexural performance of prefabricated NSC components with UHPC wet joints[D]. Changsha:Hunan University, 2018. (in Chinese)
    [19] Carbonell M A, Harris D K, Ahlborn T M, et al. Bond performance between ultrahigh-performance concrete and normal-strength concrete[J]. Journal of Materials in Civil Engineering, 2013, 26(8):04014031.
    [20] Tayeh B A, Bakar B H A, Johari M A M, et al. Mechanical and permeability properties of the interface between normal concrete substrate and ultra high performance fiber concrete overlay[J]. Construction & Building Materials, 2012, 36:538-548.
    [21] Tayeh B A, Bakar B H A, Johari M A M, et al. Evaluation of bond strength between normal concrete substrate and ultra high performance fiber concrete as a repair material[J]. Procedia Engineering, 2013, 54:554-563.
    [22] Tayeh B A, Abu Bakar B H, Megat Johari M A, et al. Microstructural analysis of the adhesion mechanism between old concrete substrate and UHPFC[J]. Journal of Adhesion Science & Technology, 2014, 28(18):1846-1864.
    [23] Harris D K, Sarkar J, Ahlborn T M. Characterization of interface bond of ultra-high-performance concrete bridge deck overlays[J]. Transportation Research Record, 2011, 2240(1):40-49.
    [24] Shafieifar M, Farzad M, Azizinamini A. Experimental and numerical study on mechanical properties of Ultra High Performance Concrete (UHPC)[J]. Construction & Building Materials, 2017, 156:402-411.
    [25] 廖肇乾. UHPC-NC界面粘结强度试验研究[D]. 长沙:湖南大学, 2018. Liao Z Q. Experimental research on bond strength of UHPC-NC interface[D]. Changsha:Hunan University, 2018. (in Chinese)
    [26] 张孝臣. 预制超高性能混凝土修复既有混凝土结构界面粘结性能研究[D]. 哈尔滨:哈尔滨工业大学, 2016. Zhang X C. Study of interface bond behavior between precast ultra high performance concrete repaired layer and existing concrete structures[D]. Harbin:Harbin Institute of Technology, 2016. (in Chinese)
    [27] 王兴旺. UHPC与普通钢筋混凝土结构界面抗剪性能研究[D]. 长沙:湖南大学, 2016. Wang X W. Research on the interfacil shear behavior of UHPC and reinforced concrete[D]. Changsha:Hunan University 2018. (in Chinese)
    [28] Anderson A R. Composite designs in precast and cast-in-place concrete[J]. Progressive Architecture, 1960, 41(9):172-179.
    [29] Birkeland P W, Birkeland H W. Connections in precast concrete construction[J]. Aci Structural Journal, 1966, 63(1):345-368.
    [30] American Concrete Institute ACI Committee. Building code requirements for structural concrete ACI 318-08 and commentary 318R-08[S]. American Concrete Institute, Farmington Hills, 2008.
    [31] AASHTO LRFD-2007, Bridge design specifications[S]. Washington D C, 2007.
    [32] CAN/CSA-S6-00 Canadian highway bridge design code[S]. CSA International, 2000.
    [33] PCI design handbook:Precast and prestressed concrete[M]. Precast/Prestressed Concrete Institute, Chicago, IL. 1999.
    [34] Fib. Fib model code for concrete structures 2010[M]. Weinheim, Germany:Wiley-VCH Verlag GmbH & Co. KGaA, 2013.
    [35] 刘杰, 陈娟娟. 新老混凝土界面抗剪强度研究现状综述[J]. 混凝土, 2015, (1):62-67. Liu J, Chen J J. State of the art review on shear strength of interface between new and old concrete[J]. Concrete, 2015, (1):62-67. (in Chinese)
    [36] Harris D K, Muñoz M C, Gheitasi A, et al. The challenges related to interface bond characterization of ultra-high-performance concrete with implications for bridge rehabilitation practices[J]. Advances in Civil Engineering Materials, 2014, 4(2):75-101.
    [37] Júlio E N B S, Branco A B, Silva V D, et al. Influence of added concrete compressive strength on adhesion to an existing concrete substrate[J]. Building and Environment, 2006, 41(12):1934-1939.
    [38] Wall J S, Ssrive N G. Factors affecting bond between new and old concrete[J]. Materials Journal, 1988, 85(2):117-125.
    [39] Ulku E, Attanayake U, Aktan H M. Rationally designed staged posttensioning to abate reflective cracking on side-by-side box-beam bridge decks[J]. Transportation Research Record, 2010, 2172(1):87-95.
    [40] Porter S D, Julander J L, Halling M W, et al. Flexural testing of precast bridge deck panel connections[J]. Journal of bridge engineering, 2010, 16(3):422-430.
    [41] Grace N, Jensen E A, Matsagar V, et al. Use of unbonded CFRP strands in transverse post-tensioning in box beam bridges[J]. International Journal of Earth Sciences and Engineering, 2012.
    [42] Grace N, Ushijima K, Baah P, et al. Flexural behavior of a carbon fiber-reinforced polymer prestressed decked bulb T-beam bridge system[J]. Journal of Composites for Construction, 2012, 17(4):497-506.
    [43] Dias-Da-Costa D, Alfaiate J, Júlio E.N.B.S. FE modeling of the interfacial behaviour of composite concrete members[J]. Construction & Building Materials, 2012, 26(1):233-243.
    [44] Chen L, Graybeal B A. Finite element analysis of ultra-high performance concrete:modeling structural performance of an aashto type Ⅱ girder and a 2nd generation pi-girder[J]. Durability, 2010.
    [45] Steinberg E, Huffman J, Ubbing J, et al. Finite element modeling of adjacent prestressed concrete box-beams[C]//Finite Element Modeling of Adjacent Prestressed Concrete Box Beams, 2013.
    [46] Hussein H H, Walsh K K, Sargand S M, et al. Modeling the shear connection in adjacent box-beam bridges with ultrahigh-performance concrete joints. I:Model calibration and validation[J]. Journal of Bridge Engineering, 2017, 22(8):04017043.
    [47] Jang H O, Lee H S, Cho K, et al. Numerical and experimental analysis of the shear behavior of ultrahigh-performance concrete construction joints[J]. Advances in Materials Science and Engineering, 2018, 2018:1-17.
    [48] 韩菊红. 新老混凝土粘结断裂性能研究及工程应用[D]. 大连:大连理工大学, 2002. Han J H. Study on fracture performance and engineering application of adherence of new and old concrete[D]. Dalian:Dalian University of Technology, 2002. (in Chinese)
    [49] 韩菊红, 赵国藩, 张雷顺. 新老混凝土粘结面断裂损伤过程区研究[J]. 工程力学, 2004, 21(6):31-35. Han J H, Zhao G F, Zhang L S. Study on fracture process zone of adhesive interface of new and old concrete[J]. Engineering Mechanics, 2004, 21(6):31-35. (in Chinese)
    [50] Corp D S S. Abaqus 6.10 analysis user's manual[M]. USA:Dassault Systèmes Simulia Corp, 2010.
    [51] GB 50010-2010混凝土结构设计规范[S]. 北京:中国建筑工业出版社, 2010. GB 50010-2010 Code for design of concrete structures[S]. Beijing:China Architecture & Building Press, 2010. (in Chinese)
    [52] 张哲, 邵旭东, 李文光, 等. 超高性能混凝土轴拉性能试验[J]. 中国公路学报, 2015, 28(8):50-58.Zhang Z, Shao X D, Li W G, et al. Axial tensile behavior test of ultra high performance concrete[J]. China Journal of Highway and Transport, 2015, 28(8):50-58. (in Chinese)
    [53] 杨剑, 方志. 超高性能混凝土单轴受压应力-应变关系研究[J]. 混凝土, 2008, (7):11-15. Yang J, Fang Z. Research on stress-strain relation of ultra high performance concrete[J]. Concrete, 2008, (7):11-15. (in Chinese)
    Related
    Cited by
    Comments
    Comments
    分享到微博
    Submit
Get Citation

欧阳娜,邓舒文. UHPC-NC组合构件界面行为研究[J].重庆大学学报,2021,44(3):63~74

Copy
Related Videos

Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:October 08,2019
  • Online: March 31,2021
Article QR Code